Cut ting edge fa i lure of sol id carbide dri l l s
Change of chip shapes in dr i l l ing
Change of chip shapes relating to cutting conditions
Photographs below show the change of chip shapes relating to change of the feed and the cutting speed. These chip shapes are
all well controlled in a proper condition range.
When the speed and feed are low, the chip shows whitish colour and the tail of the chip tends to lengthen gradually. In contrast,
as the speed or the feed increases, the chip tends to increase in brightness and becomes a compact shape with a short tail.
These changes in the shape depend on the cutting temperature. As the temperature increases, chips tend to be broken.
Flaking
(Shell-like spalling)
Irregular wear
(Irregular flank wear)
Flank wear
(Wear of cutting edge)
Feed mark
(Wear stripes in periphery)
Chipping
(Small or minute fracture
of cutting edge)
Breakage
(Relatively large fracture)
Crater wear
(Groove-like wear on rake face)
Corner wear
(Wear of peripheral corner)
Fracture
(Catastrophic breakage
of drill body)
Note: If these failures are not excessive,
the tool is in a normal condition.
High
High
Feed
Cutting speed
Low
Tail
Low
Dr i l l ing Tool s