Unknown - page 796

D204
Profile Milling
STANDARD CUTTING CONDITIONS
ISO
Workpiece material
Hardness
HB
Grade Cutting speed
Vc
(m/min)
Feed per tooth fz (mm/t)
each chipbreaker
MJ
NMJ
NAJ
Low carbon steels
C15E4, E275A, etc.
~ 200
AH725
100 - 220
0.2 - 0.7
0.17 - 0.3
-
High carbon steels
C45, C55, etc.
200 ~ 300
AH725
100 - 200
0.2 - 0.7
0.17 - 0.25
-
Alloyed steels
42CrMo4, 20Cr4, etc.
150 ~ 300
AH725
100 - 200
0.2 - 0.7
0.17 - 0.25
-
Tool steels
X40CrMoV5-1, etc.
~ 300
AH725
100 - 180
0.2 - 0.7
0.17 - 0.25
-
Stainless steels
X5CrNi18-9, X5CrNiMo17-12-3, etc.
-
AH140
90 - 180
0.2 - 0.6
0.15 - 0.25
-
Grey cast irons
250, 300, etc.
150 ~ 250
AH120
140 - 250
0.2 - 0.7
0.17 - 0.3
-
Ductile cast irons
400-15S, etc.
150 ~ 250
AH120
140 - 250
0.2 - 0.7
0.17 - 0.3
-
Aluminium alloys
Si < 13%
-
KS15F
500 - 1200
-
-
0.1 - 0.3
Aluminium alloys
Si ≥ 13%
-
KS15F
100 - 300
-
-
0.1 - 0.3
Heat-resisting alloy
Inconel 718, Ti-6Al-4V, etc.
-
AH725
20 - 50
0.2 - 0.6
0.15 - 0.25
-
· To remove excessive chip accumulation use an air blast.
· When chips stick to the cutting edges (aluminium machining),
use a water soluble cutting fluid.
· Cutting conditions are limited by machine power and material
rigidity. When the cutting width or depth is large, set Vc and fz
below the recommended values and check the machine
vibration and spindle load.