STANDARD CUTTING CONDITIONS
ISO
Workpiece material
Hardness
HB
Selection
criteria
Recommended
grade
Chip-
breaker
Cutting speed
Vc (m/min)
Feed per tooth
fz (mm/t)
Low carbon steel
C15, etc.
- 200
First choice
AH3135, AH725
MJ
100 - 250
0.1 - 0.6
- 200
Low cutting force
AH3135
ML
100 - 250
0.1- 0.5
- 200
Priority on wear
resistance
T3130
MJ
120 - 250
0.1 - 0.6
- 200
Priority on surface
quality
NS740
MJ
100 - 250
0.1 - 0.5
High carbon steel
C45, etc.
200 - 300 First choice
AH3135, AH725
MJ
100 - 230
0.1 - 0.5
200 - 300 Low cutting force
AH3135
ML
100 - 230
0.1- 0.4
200 - 300 Priority on wear
resistance
T3130
MJ
120 - 250
0.1 - 0.5
200 - 300 Priority on surface
quality
NS740
MJ
100 - 250
0.1 - 0.4
Alloyed steel
42CrMo4, etc.
150 - 300 First choice
AH3135, AH725
MJ
100 - 230
0.1 - 0.5
150 - 300 Low cutting force
AH3135
ML
100 - 230
0.1- 0.4
150 - 300 Priority on wear
resistance
T3130
MJ
120 - 250
0.1 - 0.5
150 - 300 Priority on fracture
resistance
NS740
MJ
100 - 250
0.1 - 0.4
Tool steel
X153CrMoV12, etc.
- 300
First choice
AH3135, AH725
MJ
100 - 180
0.1 - 0.5
- 300
Low cutting force
AH3135
ML
100 - 180
0.1- 0.4
- 300
Priority on wear
resistance
T3130
MJ
120 - 180
0.1 - 0.5
Stainless steel
X5CrNi18-9, etc.
-
First choice
AH3135
ML
90 - 180
0.1 - 0.4
-
Priority on fracture
resistance
AH3135, AH140
MJ
90 - 180
0.1 - 0.45
Grey cast irons
250, etc.
-
First choice
AH120
MJ
140 - 250
0.1 - 0.6
-
Priority on wear
resistance
T1215
MJ
150 - 280
0.1 - 0.6
Ductile cast iron
400-15S, etc.
-
First choice
AH120
MJ
100 - 200
0.1 - 0.6
-
Priority on wear
resistance
T1215
MJ
120 - 220
0.1 - 0.6
Aluminium alloys Si < 13%
-
First choice
TH10
AJ
500 - 1500
0.1 - 0.5
Aluminium alloys Si ≥ 13%
-
First choice
TH10
AJ
150 - 500
0.1 - 0.5
Titanium alloys
Ti-6Al-4V, etc.
-
First choice
AH3135
ML
30 - 60
0.1 - 0.4
-
Priority on fracture
resistance
AH3135
MJ
30 - 60
0.1 - 0.4
Heat-resistance alloys
Inconel 718, etc.
-
First choice
AH725
MJ
20 - 50
0.04 - 0.1
· Remove excessive chip with an air blast to prevent chip jamming.
· Use water-soluble coolant to avoid built-up edge in case extreme
welding occurs on cutting edges. (ex. aluminium machining).
· For the operation with depth of cut which varies (ex. casting skin) and ma-
chining of workpiece materials with interrupted surface, the feed (fz) should
be set to the lower recommened value shown in the above table.
· Cutting conditions may be limited depending on machine power, workpiece
rigidity, and spindle output. When the cutting width, depth or overhang
length is large, set Vc and fz to the lower recommended values and check
the machine power and vibration.