D127
Tungaloy
Face Milling
STANDARD CUTTING CONDITIONS
ISO
Workpiece material
Hardness
Priority
Recommendation
Cutting speed
Vc (m/min)
Feed per tooth
fz (mm/t)
Grade Chipbreaker
Low carbon steel
C15E, etc.
- 200 HB
First choice
AH3135
ML
100 - 300
0.2 - 0.5
- 200 HB
For wear
resistance
AH725
ML
100 - 300
0.2 - 0.5
- 200 HB
For fracture
resistance
AH140
MJ
80 - 180
0.2 - 0.5
High carbon steel
C45E, C55E, etc.
200 - 300 HB
First choice
AH3135
MJ
100 - 230
0.2 - 0.4
200 - 300 HB
For wear
resistance
AH725
MJ
100 - 230
0.2 - 0.4
200 - 300 HB
For fracture
resistance
AH140
MJ
80 - 180
0.2 - 0.4
Alloy steel
42CrMo4, 17Cr3, etc.
150 - 330 HB
First choice
AH3135
MJ
100 - 200
0.2 - 0.4
150 - 330 HB
For wear
resistance
AH725
MJ
100 - 200
0.2 - 0.4
150 - 330 HB
For fracture
resistance
AH140
MJ
80 - 150
0.2 - 0.4
Stainless steel
X5CrNi18-9, etc.
- 200 HB
First choice
AH3135
ML
100 - 150
0.1 - 0.3
Grey cast iron
250, 300, etc.
150 - 250 HB
First choice
AH120
ML
100 - 250
0.1 - 0.5
150 - 250 HB
For fracture
resistance
AH725
MJ
100 - 250
0.1 - 0.5
150 - 250 HB
For wear
resistance
T1215
MJ
150 - 300
0.1 - 0.5
Ductile cast iron
600-3, etc.
150 - 300HB
First choice
AH120
ML
80 - 200
0.1 - 0.4
150 - 300 HB
For fracture
resistance
AH725
MJ
80 - 200
0.1 - 0.4
150 - 300 HB
For wear
resistance
T1215
MJ
100 - 250
0.1 - 0.4
Hardened steel
HRC 40 - 50
First choice
AH3135
MJ
80 - 130
0.1 - 0.2
HRC 50 - 60
First choice
AH3135
MJ
50 - 70
0.05 - 0.1
ISO
Workpiece material
Hardness
Priority
Grade
Cutting speed
Vc (m/min)
Feed per tooth: fz (mm/t)
ML
HJ*
Low carbon steel
C15E, etc.
- 200
First choice
AH3135
100 - 300
0.1 - 0.5
0.5 - 2.0
- 200
For fracture
resistance
AH130
100 - 300
0.1 - 0.5
-
High carbon steel
C45E, C55E, etc.
200 - 300 HB First choice
AH3135
100 - 230
0.1 - 0.4
0.5 - 1.5
200 - 300 HB For fracture
resistance
AH130
100 - 230
0.1 - 0.4
-
Alloy steel
42CrMo4, 17Cr3, etc.
150 - 330 HB First choice
AH3135
100 - 200
0.1 - 0.4
0.5 - 1.5
150 - 330 HB For fracture
resistance
AH130
100 - 200
0.1 - 0.4
-
Stainless steel
X5CrNi18-9, etc.
- 200 HB
First choice
AH3135
100 - 150
0.1 - 0.3
0.3 - 0.7
- 200 HB
For fracture
resistance
AH130
100 - 150
0.1 - 0.3
-
Grey cast iron
250, 300, etc.
150 - 250 HB First choice
AH3135
100 - 250
0.1 - 0.5
0.5 - 2.0
150 - 250 HB For fracture
resistance
AH130
100 - 250
0.1 - 0.5
-
Ductile cast iron
600-3, etc.
150 - 250 HB First choice
AH3135
80 - 200
0.1 - 0.4
0.5 - 1.5
150 - 250 HB For fracture
resistance
AH130
80 - 200
0.1 - 0.4
-
Titanium alloy
Ti-6Al-4V, etc.
- HRC 40
First choice
AH3135
30 - 60
0.1 - 0.3
0.3 - 0.7
- HRC 40
For fracture
resistance
AH130
30 - 60
0.1 - 0.3
-
Heat resistant alloy
Inconel718, etc.
- HRC 40
First choice
AH3135
10 - 40
0.05 - 0.15
0.1 - 0.3
- HRC 40
For fracture
resistance
AH130
10 - 40
0.05 - 0.15
-
Hardened steel
HRC 40 - 50
First choice
AH3135
80 - 130
-
0.1 - 0.3
HRC 50 - 60
First choice
AH3135
50 - 70
-
0.03 - 0.07
* Apply 20% of recommended feed when using HJ insert with ap over 1.5 mm.