Unknown - page 904

D312
Multi Function
MACHINING DATA FOR SOLID CARBIDE ENDMILLS
ISO
Material
Condition
Tensile
Strength
(N/mm2)
Hardness
HB
Cutting speed: Vc (m/min)
min
max
Non-alloy steel
and cast steel,
free cutting steel
< 0.25 %C
Annealed
420
125
220
230
≥
0.25 %C
Annealed
650
190
170
190
< 0.55 %C Quenched and tempered
850
250
140
150
≥
0.55 %C
Annealed
750
220
140
150
≥
0.55 %C Quenched and tempered
1000
300
120
130
Low alloy steel
and cast steel
(less than 5% all elements)
Annealed
600
200
140
150
Quenched and tempered
930
275
100
110
Quenched and tempered
1000
300
110
120
Quenched and tempered
1200
350
120
130
High alloy steel,
cast steel, and tool steel
Annealed
680
200
110
130
Quenched and tempered
1100
325
60
70
Stainless steel and cast steel
Ferritic / martensitic
680
200
100
170
Martensitic
820
240
60
150
Austenitic
600
180
70
100
Cast iron nodular (GGG)
Ferritic / pearlitic
-
180
70
220
Pearlitic
-
260
110
200
Grey cast iron (GG)
Ferritic
-
160
130
230
Pearlitic
-
250
70
230
Malleable cast iron
Ferritic
-
130
130
230
Pearlitic
-
230
110
200
Aluminium-wrought alloy
Not cureable
-
60
670
700
Cured
-
100
610
690
Aluminium-cast, alloyed
≤
12% Si
Not cureable
-
75
670
700
Cured
-
90
610
690
> 12% Si
High temperature
-
130
270
280
Copper alloys
> 1% Pb
Free cutting
-
110
330
350
Brass
-
90
330
350
Electrolitic copper
-
100
230
250
Non-metallic
Duroplastics, fiber plastics
-
-
-
-
Hard rubber
-
-
-
-
High temp. alloys
Fe based
Annealed
-
200
20
30
Fe based
Cured
-
280
20
20
Ni or Co based
Annealed
-
250
20
20
Ni or Co based
Cured
-
350
20
20
Ni or Co based
Cast
-
320
30
60
Titanium and Ti alloys
RM 400
-
30
60
Alpha + beta alloys cured RM 1050
-
30
60
Hardened steel
Hardened
-
55 HRC
30
40
Hardened
-
60 HRC
30
30
Chilled cast iron
Cast
-
400
50
60
Cast iron
Hardened
-
55 HRC
30
40